I want to try parts of Cyb's Max Ion Tek while still using the q21q21 dry tek.
I normally do q21q21 which starts with a warm vinegar soak.
Max Ion starts with freeze-thaw, then acid. Any reason not to hydrate the bark with vinegar in the first place and freeze-thaw it while acidified? Vinegar lowers surface tension and acts like a wetting agent; perhaps that would help get the water into the cells so freeze-thaw is more effective.
Can salting the calcium hydroxide mud help the yield or separation of solvent in the same way as salting a lye solution?
I normally do q21q21 which starts with a warm vinegar soak.
Max Ion starts with freeze-thaw, then acid. Any reason not to hydrate the bark with vinegar in the first place and freeze-thaw it while acidified? Vinegar lowers surface tension and acts like a wetting agent; perhaps that would help get the water into the cells so freeze-thaw is more effective.
Can salting the calcium hydroxide mud help the yield or separation of solvent in the same way as salting a lye solution?